Low-Carbon Aluminium Extrusions: What Buyers Should Verify Before Accepting a Carbon Figure - Siken Aluminum

Low-Carbon Aluminium Extrusions: What Buyers Should Verify Before Accepting a Carbon Figure

Two numbers now arrive with the quotation

An aluminium extrusion quotation used to argue about alloy, temper, tolerance and lead time. Today a second envelope arrives with it: recycled content in percent, and embodied carbon in kilograms of CO2 equivalent per kilogram of profile. Both figures are easy to print on a letterhead and hard to verify, and both are now asked for by buyers who have to report them upward.

This note is about the second part: what can actually be checked before a carbon claim enters a purchasing file, and which claims collapse under inspection.

Recycled content is a mass-balance claim, not a material property

Aluminium is not tagged. Once a remelt furnace charges primary ingot, process scrap and post-consumer scrap into the same bath, the metal leaving the casting table has one chemistry and no memory of where it came from. A statement of “60% recycled” therefore describes a bookkeeping method, not a property of the bar you receive.

Two methods dominate. The first is mass balance along a chain of custody: the input mix is averaged over a defined period and production unit. The second is book-and-claim: recycled content is purchased as certificates and attributed to a product line. Both are legitimate when they are declared. Neither means that every kilogram delivered contains that percentage of scrap.

What secondary billet changes inside the press

Alloy chemistry is controllable; trace elements are not free. Scrap carries iron, zinc, lead and coating residues into the melt. A 6063 billet built from selected process scrap and clean post-consumer extrusion behaves much like primary metal. A billet that includes painted, anodized or mixed shred scrap needs more dilution, more degassing and finer filtration to reach the same specification.

In the press, higher iron raises flow stress slightly and accelerates die wear. The larger effect is inclusion load: alumina, spinel and undissolved intermetallics disturb metal flow at the bearing, and that is where surface defects begin. Cleanliness is a melting and casting property, not something the extrusion line can add later.

Where scrap-heavy billet shows up on the finished profile

Usually not in the mill finish, and rarely in the mechanical test certificate. It appears after anodizing: faint longitudinal streaks, a milky or patchy etch, colour variation between profiles from different billet batches, or a seal quality test that fails near the ends. Each of these points back to billet cleanliness or homogenisation.

For a mill-finish heat sink or a powder-coated machine frame, the same billet may be perfectly acceptable. The requirement should follow the finish and the application, not a general preference for greener metal.

What a carbon figure has to declare

An embodied-carbon number without a system boundary is not a number. At minimum the declaration should state whether the boundary is cradle-to-gate or cradle-to-grave; whether electricity is metered or modelled, and at which grid factor; whether the billet was cast in the same plant as the extrusion or bought in; how scrap allocation was handled; and which standard the calculation follows — an EPD under EN 15804, a product carbon footprint to ISO 14067, or a customer-specific protocol.

Ask for the calculation as a document, not a slide. One page of stated assumptions is worth more than two decimal places.

Same drawing, two different answers

Claim What it actually means What supports it
“70% recycled content” An averaged input mix, or certificate-backed attribution, for a defined period Mass-balance statement with period, production unit and scrap categories
“Low-carbon billet” Lower embodied carbon per kilogram, typically from hydro or renewable electricity rather than more scrap Supplier EPD or PCF with grid factor and energy source declared
“Primary quality from recycled metal” Chemistry and inclusion level held to the alloy specification, not a statement about the input Spectro report per cast, degassing and filtration records, anodizing coupon
“Carbon neutral profile” Emissions reduced inside the product system, with the remainder offset outside it Reduction evidence first, then the offset instrument and its retirement record
“CBAM ready” Embedded emissions reported in the structure the EU importer has to file Installation-level data, CN code, production route and a verifiable calculation method

Why two suppliers quote different intensity for the same drawing

Three legitimate reasons. Electricity: a smelter on hydroelectric power and an extruder on a coal-heavy grid are not describing the same kilogram. Boundary: one figure covers billet, extrusion and anodizing, another covers extrusion only with customer-supplied billet. Allocation: how scrap credit is divided between the product that generated the scrap and the product that consumes it moves the result by a wide margin.

Compare only after all three are aligned. A lower number produced by a narrower boundary is not a better profile.

The regulatory layer, briefly

Since 2026 the EU Carbon Border Adjustment Mechanism has applied to aluminium in its definitive period. Importers report embedded emissions, and the first annual declaration, covering goods imported during 2026, falls due by 30 September 2027. The practical consequence for a buyer sourcing from China is documentary: the emissions figure has to be installation-specific and defensible, not an industry average copied into a template.

The alloy question: when recycled ratio is not the constraint

For 6063 architectural and heat-sink profiles, a well-controlled secondary billet is often indistinguishable in service. For 6061 structural work, or for parts that will be hard anodized to a 20 µm class and sealed, the limits tighten: iron at or below 0.35%, silicon inside 0.20–0.60%, and a hydrogen level that will not open porosity during the die trial.

That is a chemistry requirement, not a recycling requirement. A supplier who meets it from secondary metal is doing better work than one who meets it by diluting with primary — but only the inspection record shows which of the two actually happened.

A verification checklist for the purchasing file

  • Mass-balance statement naming the period, the production unit and the scrap categories included.
  • Carbon calculation with boundary, grid factor, energy source and the standard cited.
  • Spectro report for the cast actually used on your order, not a generic alloy certificate.
  • Anodizing coupon from the same billet batch, if the profile is to be anodized.
  • One trial order before the figure is used in your own Scope 3 reporting.

What we do not claim

We do not claim that a recycled-content percentage guarantees a lower footprint for your specific order, and we do not convert an industry average into a product figure. What we can put in writing is the billet source, the chemistry per cast, the anodizing result and the calculation method, so that the number in your report is one you can defend.

Send the alloy, the finish and the destination market. We will say which parts of the carbon file we can support with documents, and which parts we cannot.

Category: Technical Guide

Leave a Comment

Your email address will not be published. Required fields are marked *